3M 233 PLUS
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Conformable Automotive Paint Masking
- Defined ASTM Physical Strength
- Short High-Temperature Exposure
Product Description
Scotch Masking Tape 233 is a smooth mini-crepe paper masking tape with a proprietary rubber-based adhesive for automotive refinish paint masking. Its balanced construction combines instant adhesion and holding power with conformability around curves and controlled handling during application. Typical physical data include 8.0 mil (0.20 mm) thickness, 30 lb/in tensile strength, and 12% elongation at break. The tape resists solvent and moisture, provides clean removal under supported conditions, and tolerates up to 250 deg F (121 deg C) for 30 minutes. It is used for masking cars, airplanes, boats, and trucks where crisp paint lines and reliable edge control are required.
Key features
- Conformable mini-crepe backing: The smooth paper backing follows curves and contours while supporting controlled hand application.
- Defined physical strength: Typical tensile strength is 30 lb/in with 12% elongation at break under ASTM D3759.
- Short high-temperature exposure: The tape tolerates up to 250 deg F (121 deg C) for up to 30 minutes.
Applications
Applications include automotive refinish paint masking on cars, airplanes, boats, and trucks.
TDS, SDS & Technical Documents
Technical Specifications
Mechanical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Physical values are typical unless the method / condition states otherwise.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Backing | Smooth mini-crepe paper | - | As supplied |
| Adhesive | Proprietary rubber-based | - | As supplied |
| Total thickness | 8.0 (0.20) | mil (mm) | Typical; ASTM D3652 |
| Tensile strength | 30 | lb/in width | Typical; ASTM D3759 |
| Elongation at break | 12 | % | Typical; ASTM D3759 |
| Shelf life | 12 | months | From manufacture; original carton at 60 to 80 deg F and 50% RH |
Final-state / after-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesion to steel | 40 | oz/in width | Typical; ASTM D3330 |
| Temperature use | Up to 250 (121) | deg F (deg C) | Up to 30 min |
| Clean-removal period | Up to 5 | days | Applied tape |
| Solvent and moisture resistance | Good | - | Applied tape backing |