3M Electrically Conductive Double-Sided Tape 9793KT Series

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M Electrically Conductive Double-Sided Tape 9793KT Series

Main features

  • Typical Z-axis electrical resistance`
  • Typical expected shielding effectiveness is 40-60 dB
  • Ten thicknesses from 130 to 500 µm

Product Description

3M-9793KT is an XYZ-axis electrically conductive double-sided pressure-sensitive adhesive tape that combines conductive acrylic PSA with a porous conductive foam matrix. The tape creates an adhesive electrical path between joined substrates and is used in grounding and EMI shielding in equipment and electronic components. Ten thickness variants from 130 to 500 µm provide options for different assembly geometries, with a transparent PET release liner supplied for handling before application. Product selection should consider thickness, adhesion target, surface condition and the pressure needed to develop sufficient adhesive contact and electrical connection.

Key features

  • XYZ-axis conductive construction: Conductive acrylic PSA and a porous conductive foam matrix form the electrically conductive tape structure.
  • Z-axis electrical resistance: 0.01-0.25 Ω under 3M ETM-12 test conditions.
  • EMI shielding performance: Typical expected shielding effectiveness of 40-60 dB through the tape thickness using standard EMI shielding test methods.
  • Thickness range: Ten variants from 130 to 500 µm support different assembly geometries.
  • Adhesion to stainless steel: Face- and back-side target values range from 1000 to 2500 gf/inch by thickness under ASTM D1000.

Applications / Suitable for

  • Grounding between conductive substrates.
  • EMI shielding in equipment.
  • Conductive pressure-sensitive attachment in electronic components.
Product Family

234983

9793KT-300 | 480mm × 50m
1. Select Width
2. Select Length
3. Select Version

Loading pricing…

Packaging
Please select Width, Length and Version.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Acrylic Adhesive Conductive Foam Matrix
Color
The color
Grey Metallic
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
Transparent PET Release liner

Additional Information

Electrically Conductive Tapes

3M-9793KT

3M-9793KT is an XYZ-axis electrically conductive double-sided pressure-sensitive adhesive tape built with a conductive acrylic adhesive and porous conductive foam matrix. It combines adhesive attachment with an electrical path between joined substrates for grounding and EMI shielding in equipment and electronic components. The series offers ten thicknesses from 130 to 500 µm to support different assembly geometries.

XYZ-axis electrical conductivity Double-sided PSA Conductive foam matrix 10 thickness variants: 130-500 µm

3M-9793KT electrically conductive double-sided pressure-sensitive adhesive tape.

Product construction

Construction and as-supplied characteristics

Construction
Conductive acrylic PSA + porous conductive foam matrix
The conductive adhesive and carrier form the double-sided tape structure used to attach to grounding surfaces.
Color
Grey metallic
The face and back sides are both listed as grey metallic.
Release liner
Transparent PET
The tape is supplied with a transparent PET release liner for handling before application.

Thickness and adhesion options

The 9793KT series is offered in ten thickness variants. Face- and back-side adhesion targets to stainless steel are identical for each listed variant, allowing thickness and the corresponding adhesion target to be reviewed together during initial selection.

Variant Thickness (µm) Adhesion to SUS, face/back (gf/inch) Selection note
9793KT-130 130 1000 Lowest listed thickness; 1000 gf/inch target adhesion.
9793KT-150 150 1800 150 µm option; 1800 gf/inch target adhesion.
9793KT-180 180 1800 180 µm option; same 1800 gf/inch target adhesion.
9793KT-210 210 2000 210 µm option; 2000 gf/inch target adhesion.
9793KT-230 230 2000 230 µm option; 2000 gf/inch target adhesion.
9793KT-255 255 2000 255 µm option; 2000 gf/inch target adhesion.
9793KT-300 300 2500 300 µm option; 2500 gf/inch target adhesion.
9793KT-350 350 2500 350 µm option; 2500 gf/inch target adhesion.
9793KT-400 400 2500 400 µm option; 2500 gf/inch target adhesion.
9793KT-500 500 2500 Thickest listed option; 2500 gf/inch target adhesion.

Adhesion values are target/typical data measured to stainless steel in accordance with ASTM D1000 and are not specification limits.

Application guidance

Application and bonding process

Bond strength depends on adhesive-to-surface contact, substrate type and surface condition. Firm pressure after assembly is also used to develop wet-out and engage the conductive adhesive with the substrates to establish electrical connection. Pressure, dwell time and moderate heat are process variables to evaluate for the specific assembly.

Application temperature: Tape application below 10°C (50°F) is not suggested.
Surface preparation: Bonding surfaces should be clean, dry and well unified. Isopropyl alcohol or heptane are cited as typical cleaning solvents; follow the solvent manufacturer's precautions and directions for use.
Pressure and dwell: Apply 5-15 psi after assembly using a roller, metal bar or finger pressure. A suggested initial DOE range is 5-15 psi for 2-5 seconds at 21-38°C.
Optional heat: Heat in the 38-60°C range may be evaluated simultaneously with pressure to improve wetting, final bond strength and electrical conductivity.
Adhesion build: Up to 24-72 hours may be required to reach final adhesion values.


Firm pressure after assembly develops adhesive contact and engages the conductive adhesive with the substrates.

Storage and Handling

Shelf life is 12 months from the date of manufacture when the tape is stored in roll form, in its original packaging, at 10-25°C (50-77°F) and less than 60% relative humidity. After removal from the original packaging, converted, shipped and stored material should remain within the prescribed temperature and humidity controls. If the release liner is exchanged during converting, test the replacement liner with the tape; transferred release agents can reduce tack, adhesion, electrical performance and shelf life.

Final performance

Electrical and EMI performance

Values shown are representative/typical and are not specification limits. Electrical resistance and shielding performance depend on contact and test conditions.

Property Value Unit Method / condition
Z-axis electrical resistance 0.01-0.25 Ω 3M ETM-12; 10 mm x 10 mm contact area, one pass with a 2 kg rubber roller, 20-minute dwell, then DC resistance measurement.
Shielding effectiveness 40-60 dB Typical expected range through the tape thickness using standard EMI shielding test methods. Result depends on conductive-layer construction, adhesive contact, surface smoothness and test frequency.
Next steps

Discuss your conductive tape application

Contact Krayden to discuss 3M-9793KT thickness selection, grounding paths, surface preparation, application pressure, converting requirements and integration into EMI shielding assemblies. The team can review the process variables and interface conditions relevant to your intended use.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers