3M DP460

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M™ Scotch-Weld™ 460

Main features

  • High shear strength
  • 60-minute work life
  • Easy mixing

Product Description

3M™ Scotch-Weld™ Epoxy Adhesives DP460 is a high performance, two-part epoxy adhesive offering outstanding shear and peel adhesion, and very high levels of durability.

Product Key Features

  • High shear strength
  • 60 minute work life
  • Easy mixing
  • High peel strength

Applications

  • Structural bonding of metals, composites, and plastics
  • Automotive and transportation assemblies
  • Aerospace interior and non-critical structural components
  • Bonding panels, brackets, and enclosures
  • Industrial equipment fabrication and repair
  • Electronics housing and component assembly
  • General-purpose maintenance and manufacturing bonding
Product Family

3M DP460

1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
20,000-50,000 mPa.s
General Properties
Color
The color
white/amber
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
2:1
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
60 minutes hours
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.18 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2.4e+14 Ohms⋅cm