ABLESTIK 563K

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK 563K

Main features

  • Good heat transfer
  • Low squeeze out
  • Thermally conductive

Product Description

LOCTITE ABLESTIK 563K epoxy adhesive film is suitable for bonding "hot" devices onto heat sinks where electrical insulation and good heat transfer are required. It exhibits low squeeze out during bonding. This product provides high strength over a wider temperature range than is normally associated with flexible films.

LOCTITE ABLESTIK 563K  is a thermally conductive film with good heat transfer which manages to achieve a thin bondline with uniform bondline control. It comes without a carrier and is typically available in 50um and 75um microns.

 

Cure Schedule

  • 30 minutes @ 150°C
  • 2 hours @ 125°C
Product Family

213490

003 | 6 in x 6 in - Sheet
1. Select Package Type
2. Select Thickness

Loading pricing…

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Unit of measure Box
Net weight 3.263 g
Gross weight 3.263 g
Dimensions 15.2 x 15.2 x 0 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
2160 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
97 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.1 W/m.K

Additional Information

Outgassing

NASA Outgassing:

  • TML, % 0.44
  • CVCM, % 0.04
  • WVR, % 0.2

Leading Brands Trust in Our Products and Services