ABLESTIK 56C
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- High bond strength
- Very low temperature cure
- Passes NASA ougassing
Product Description
LOCTITE ABLESTIK 56C adhesive is designed to make electrical connections where hot soldering is impractical or to make electrical connections to conductive plastics at locations which cannot be subjected to high temperatures.
LOCTITE ABLESTIK 56C can be used with a variety of catalysts. For more information on mixed properties when used with other available catalysts, please contact your local technical service representative for assistance and recommendations.
LOCTITE ABLESTIK 56C in the CAT 9 KIT is used in a 100:2.5 ratio and passes NASA outgassing standards. The specifications in this page are for the cured CAT9 mix. It is an assembly two component adhesive that works on metals, glass, ceramic and plastic surfaces with an operating temperature of -60 to 120°C.
Cure Schedule
- 2 hours @ 50°C