ABLESTIK 8370
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Gold Filled
- High electrical conductivity
- Works on Noble finished substrates
Product Description
LOCTITE ABLESTIK 8370 adhesive is designed for automatic dispensing operations, where silver migration is a concern.
LOCTITE ABLESTIK 8370 is a dispensable gold filled adhesive than can replace Silver filled alternatives when migration is not acceptable at all. It is compatible with Noble substrate finishes and should not be used in Sn terminations. Even though Silver migration is unlikely to happen in ovemolded packages, there are certain applications that can be susceptible to it such as Automotive LED and that is where this high cost and high performance product shines.
Cure Schedule
- 1 hour @ 150°C