MM211 | Maleimide adhesion promoter Additive

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

MM211 | Maleimide adhesion promoter Additive

Main features

  • Adhesion promoter
  • Flexible aliphatic backbone
  • Maleimide and carboxylic groups

Product Description

MM-211 is an intermediate chain length, maleimide, terminated carboxylic acid. It is a useful intermediate for the synthesis of ester and amide linked thermoset monomers. The alkyl chain provides flexibility and hydrophobicity.

MM-211 is recommended for use as a synthetic intermediate for maleimide functional resins. It may also be used as an adhesion promoter in free-radical or epoxy/(meth)acrylate hybrid adhesives to bind on metal surfaces.

 

Product Family

233505

50gr Sample Jar
1. Select Package Type

Loading pricing…

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Unit of measure Jar
Net weight 0.05 kg
Gross weight 0.24 kg
Dimensions 6 x 6 x 13 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White powder