DOWSIL 732

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 732 MULTI-PURPOSE SEALANT

Main features

  • One-Part Moisture-Cure Sealing
  • Thermal Stability for Sealing
  • Non-Sag Placement Control

Product Description

DOWSIL™ 732 Multi-Purpose Sealant is a one-part, general-purpose silicone adhesive and sealant. It utilizes an acetoxy cure system to cure at room temperature when exposed to atmospheric moisture, forming a tough, flexible rubber. Available in white, black, clear, and aluminum, it features a non-sag paste consistency that makes it easy to apply for various bonding and sealing needs.

Product Key Features

  • One-Part Moisture Cure - cures at room temperature upon exposure to moisture in the air, offering a skin-over time of 7 minutes and a tack-free time of 20 minutes.
  • Thermal Stability - remains stable and flexible from -60°C to +180°C, with short peaks up to +205°C[cite: 1595, 1596]. The black version offers extended stability up to +205°C, with short peaks up to +230°C.
  • Mechanical & Electrical Profile - delivers a Shore A hardness of 25, a tensile strength of 2.3 MPa, an elongation of 540%, and excellent dielectric properties.
  • Regulatory Compliance - complies with MIL-A-46106 and FDA 177.2600 specifications.
  • Non-Sag Rheology - maintains a non-slump paste consistency, ensuring it remains in place during application.

Applications

This sealant is ideal for general industrial sealing and bonding applications where a durable, flexible rubber seal is required.

  • General Industrial Bonding - provides good, unprimed adhesion to many substrates such as glass, metals, and most common engineering plastics.
  • High-Temperature Environments - suitable for assemblies experiencing extreme temperature fluctuations requiring continuous thermal stability.
  • Regulated Applications - can be confidently used in settings requiring compliance with FDA 177.2600 or MIL-A-46106 standards.

Technical Specifications

General Properties
Color
The color
White, black, clear or aluminum
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.04
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
821,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
540 %
Physical Properties
Skin Time
7 minutes
Tack-Free Time
20 minutes
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
21.6 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.5e15 Ohms⋅cm

Additional Information

General Purpose Silicone Adhesive / Sealant

DOWSIL™ 732 Multi-Purpose Sealant

DOWSIL™ 732 Multi-Purpose Sealant is a premier one-part silicone adhesive and sealant engineered for a diverse range of general industrial sealing and bonding applications. Operating via an acetoxy moisture-cure mechanism, this non-sag paste cures efficiently at room temperature upon exposure to atmospheric moisture, transforming into a tough, highly flexible silicone rubber. It provides excellent dielectric properties, stable performance across wide temperature configurations, and robust unprimed adhesion to many common substrates. Fully compliant with military specification MIL-A-46106 and FDA 177.2600 regulations, it ensures long-term joint reliability for demanding manufacturing and maintenance frameworks.

One-part moisture cure 7 min skin-over time MIL-A-46106 Compliant FDA 177.2600 Compliant
Contact Us

Typical values only. Performance metrics are measured following full moisture activation under standard room temperature settings.

DOWSIL 732 Multi-Purpose Sealant product package
DOWSIL™ 732 Multi-Purpose Sealant

Key Features

  • One-part RTV formulation requires no pre-mixing equipment, optimizing factory process lines and minimizing waste.
  • Thixotropic non-sag paste consistency tracks cleanly and stays in place on vertical or overhead joints.
  • Cures to a tough, highly flexible silicone rubber capable of resolving substrate thermal expansion differentials.
  • Excellent unprimed adhesion profiles over glass, ceramics, common metals, and engineering plastics.
  • Outstanding dielectric performance parameters coupled with high volume resistivity (1.5x10¹⁵ Ohm-cm).
  • Certified to meet military specification MIL-A-46106 and FDA 177.2600 food-contact criteria.

Processing Summary

Color Assortment: Produced in a versatile industrial palette of white, black, clear, and aluminum variants to perfectly coordinate with design aesthetics.
Skin-Over & Tack Windows: Surface skin formation starts rapidly in 7 minutes at 25°C. Transitions to a complete tack-free state within 20 minutes. Tooling should be completed with a spatula before skinning occurs.
Inward Cure Progress: Cross-linking moves inward from the exposed surface at 25°C and 50% RH, achieving a cure depth of roughly 3 mm within 24 hours. Confinement or lower humidity extends this duration.
Thermal Endurance Profiles: Standard configurations maintain flexibility from -60°C to 180°C with short peaks to 205°C. The black version delivers enhanced resistance from -60°C to 205°C with peaks to 230°C.
Handling and Application Guidance

Process Notes 

Storage and Shelf Life
  • Store raw materials at or below 32°C (90°F) in original, unopened containers.
  • Keep containers tightly closed when not in use, as the product cross-links via reaction with air moisture.
  • A cured plug of material may form in the nozzle tip during storage; this is easily removed and does not harm contents.
  • Track stock rotation based on the formal "Use Before" date printed on the container labels.
Surface Preparation
  • Joint boundaries must be completely clean and dry prior to sealant extrusion.
  • Degrease and clear contaminants using isopropyl alcohol, acetone, or methyl ethyl ketone (MEK).
  • While unprimed adhesion is excellent on glass and metals, it will not normally bond to PTFE, PE, or PP.
  • For maximum adhesion, wipe with solvent, then apply a thin coat of DOWSIL™ 1200 OS Primer and let dry for 15-90 minutes.
Substrate Compatibility Note
  • The acetoxy cure chemistry releases a small amount of acetic acid vapor as a by-product during vulcanization.
  • This acetic acid byproduct can potentially cause corrosion on certain sensitive metallic parts or sub-assemblies.
  • Avoid processing this sealant inside totally enclosed or confined configurations where vapor by-products cannot escape.
  • Before handling and packaging parts, allow a sufficiently long dwell time to protect adhesive seal integrity.
Typical Properties

Engineering Data for DOWSIL™ 732

Uncured Physical Properties 

Physical Property Typical Engineering Value Corporate Test Method (CTM) / Condition
Appearance Non-slump paste CTM 0176
Color Assortment White, black, clear, or aluminum CTM 0176
Extrusion Rate 350 g/minute Measured using 3.2 mm orifice at 0.62 MPa (CTM 0364)
Viscosity (Low Shear - 1/s) 821 Pa-sec CTM 1377
Viscosity (High Shear - 10/s) 168 Pa-sec CTM 1377

Cured Mechanical & Electrical Properties

Properties measured following a full 7-day cure in air at 25°C (77°F) and 50% relative humidity.

Elastomeric Parameter Typical Engineering Value Test Standard Basis (ASTM / CTM)
Specific Gravity 1.04 ASTM D1475 / CTM 0097B
Durometer Hardness 25 Shore A ASTM D2240 / CTM 0099
Tensile Strength 2.3 MPa ASTM D412 / CTM 0137A
Elongation at Break 540 % ASTM D412 / CTM 0137A
Volume Coefficient of Thermal Expansion 1.12 x 10⁻³ 1/K CTM 0420
Dielectric Strength 21.6 kV/mm ASTM D149 / CTM 0114
Dielectric Constant (Permittivity) 2.8 Evaluated at 100 Hz to 100 kHz (ASTM D150 / CTM 0112)
Dissipation Factor 0.0015 Evaluated at 100 Hz to 100 kHz (ASTM D150 / CTM 0112)
Volume Resistivity 1.5 x 10¹⁵ Ohm-cm ASTM D150 / CTM 0112
Applications

Where DOWSIL™ 732 Fits

General industrial factory sealing and component bonding
Industrial Sealing & Bonding
Perfect for a vast array of general multi-material manufacturing joins and maintenance procedures across production facilities.
  • Ready-to-use general purpose silicone paste adhesive.
  • Bonds tight to glass, metals, and engineering plastics.
  • Easy toolability with a spatula for neat, aesthetic beads.
Regulated industrial equipment assembly sealing
Regulated Assemblies
Extensively tested and recognized under international agency standards to support highly specific defense and commercial guidelines.
  • Fully complies with military standard MIL-A-46106.
  • Meets strict FDA 177.2600 food-contact criteria.
  • Ensures strict material tracking and verified compliance.
Flexible thermal expansion stress relief sealing
Thermal & Flexible Joints
Forms a tough, flexible rubber skin with 540% elongation to accommodate structural movements and mechanical vibrations.
  • Excellent environmental sealing and moisture blocking.
  • Dielectric breakdown protection tracks at a strong 21.6 kV/mm.
  • Absorbs relative shifting between dissimilar joint materials.
Product Demo

See One-Part Moisture-Curing Silicone Paste Dispensing Methods

Observe the high-precision processing of one-part non-flowing general-purpose silicone adhesive sealants via automated needle dispensing setups. This practical reference highlights best practices for balancing track extrusion parameters, checking non-slump bead profiles, and verifying surface handling stability before complete room temperature cross-linking completes.

Package & Support

Standard Packaging & Technical Help

Standard Packaging
  • Available across multiple standard industrial container net weight classes.
  • Supplied ready-to-use for direct extrusion without multi-part manual blending steps.
  • Packaging configurations safeguard raw material against air moisture contamination.
Technical Help Capabilities
  • Assisting manufacturing loops with room-temperature setup to bypass thermal oven operating costs.
  • Evaluating substrate material groups to optimize unprimed dính bám on engineering plastics.
  • Configuring automated needle dispensing parameters to coordinate with the specified 350 g/min extrusion rate.
  • Providing formal compliance certificates and safety parameters verifying MIL and FDA approvals.
Technical Guidance

Tips and Troubleshooting

Issue Recommended Action
Premature layer skinning or surface tearing during finishing tooling steps
  • Surface skin over progresses fast, typically commencing within 7 minutes at standard parameters.
  • Ensure any smoothing adjustments or spatula profiling operations are completed before the surface skin initializes.
  • Perform assembly line joins immediately after application to guarantee complete adhesive transfer across boundaries.
Incomplete structural cross-linking down through joint core zones
  • One-part moisture cure chemical cross-linking relies strictly on atmospheric moisture and progresses inward from the exterior skin.
  • Do not utilize this multi-purpose product in highly confined or enclosed pockets lacking proper air access.
  • Be aware that deep-section cure dimensions advance at an approximate depth tracking rate of 3 mm per 24 hours.
  • Expect extended cure tracking behaviors if the plant floor surrounding relative humidity indices fall low.
Adhesion tracking breakdown or low lap shear force values over difficult substrates
  • Unprimed structural bonds will not stick successfully onto non-reactive substrates like Teflon, polyethylene, or polypropylene.
  • Highly plasticized plastics or rubbers can leach mobile components over time, which function as active release agents.
  • Verify all targets are cleanly washed of mill fluids or grease using isopropyl alcohol, acetone, or MEK.
  • Apply specialized surface configurations such as chemical etching, inline plasma treatment, or compatible DOWSIL™ Primers.
Next Steps

Ready to Qualify DOWSIL™ 732?

Tell us about your performance, design, and manufacturing challenges. Share your specific substrate pairings, joint geometry designs, takt time constraints, and environment parameters. Our global technical support team is prepared to put our silicon-based material expertise and process knowledge to work for your production floor.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers