Hysol GR700 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR700 | Black Epoxy Mold Compound

Main features

  • Low stress
  • For high power devices
  • Good electrical performance

Product Description

Hysol GR700, is a halogen free, black, silica filled (87% filler weight) semiconductor grade green epoxy molding compound designed for SOP MSL1. This low stress, high adhesion compound has very good electrical performance and is a proven, commercially available product code. This is a product that has achieved MSL 1 and its comparative tracking index (CTI) is 600V.

Hysol GR700 is a technologically advanced, halogen free, green epoxy molding compound with excellent electrical performance, designed for high power devices applications with low moisture absorption requirements. Typical use can be in SOP, DPAK,QFP, QFN, SOT semiconductor packages. Furthermore, it meets UL 94 V-0 flammability at 1/8 inch thickness..

HYSOL GR700 has been formulated to provide the best possible moldability and as wide a molding latitude as possible. Although molding and curing conditions will vary from situation to situation.


Available versions:

Product Family

233944

Pelletized - 14MM X 4.4GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm

Technical Specifications

General Properties
Color
The color
Black
Filler Content
87 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.97
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
118 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.9 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
60E15 Ohms⋅cm
Chemical Properties
Moisture absorption
0.26 %
Physical Properties
Spiral Flow @ 175°C
132.08 cm
Mechanical Properties
Molded Shrinkage
0.2 %
Curing Conditions
Transfer Pressure
40-85 kg/cm2
Transfer Time
8-15 s

Additional Information

GR700 Series for High-reliability Small Outline Packages