WS300 | Wax Conditioning Sheets

Harmonization Code : 4005.91.00.00 | Compounded rubber, unvulcanized, in primary forms or in plates, sheets or strip: Plates, sheets, and strip

WS300 | Wax Conditioning Sheets

Main features

  • Carcinogen free
  • Excellent workability
  • Good self release

Product Description

WS300 Waxed Rubber Conditioning sheets are used to protect the mold surface and ensure a good releasing effect after cleaning. It has a low to medium viscosity and is intended for IC & Discrete application processes.

WS300 is a carcinogen free self releasing sheet with excellent workability and good fluidity with minimal odor. It can fill deep cavities and exhibits great self release properties. This sheet which is mainly used for compression mold conditioning cures in ~300-600seconds and can requires 1-2 shots. It can withstand pressure between 30-130 psi and a mold temperature range of 165-200°C.

WS300 can be used in various steps of the cleaning and conditioning processes, either in normal cleaning or in enhanced, prolonged or mid term conditioning. It is always 1-2shots right after the cleaning process unless it is used for mid term where it can condition the mold right after the second, intermediate production run.

For reference, a normal EMC cleaning process would go as follows:

  1. Production
  2. Cleaning with Rubber cleaning sheets
  3. Conditioning with Wax conditioning sheets
  4. Dummy EMC molding
  5. Production
  6. Proverbially Rinse and repeat
Product Family

233209

1 kg | 230mm x 7mm - 10mm Slot - Width 250mm | MELF Diodes
1. Select Width
2. Select Sheet Size
3. Select Package Type
4. Select Length
5. Select Thickness
6. Select Slot Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Box
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 24 x 25 x 1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Light Gray
Compression Pressure
30 - 130 Kg/cm2
Other Properties
Shots
1-2

Additional Information

A normal cleaning and conditioning Cycle for Diodes is:

5 shots of the RCS400 - Diodes cleaning + 2 shots of the WS300 - Diodes conditioning sheets