LOCTITE 580

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite 580 Pipe Sealant

Main features

  • One-Component Sealing System
  • Low Pressure Sealing for Inactive Metals
  • Room-Temperature Sealing Cure

Product Description

LOCTITE® 580 is a one-component, very-high-viscosity anaerobic thread sealant designed for locking and sealing close-fitting metal pipes and fittings. The off-white methacrylate paste provides lubricity during assembly, supports immediate low-pressure sealing in properly tightened fittings, and cures without heat when confined between metal threaded surfaces.

Key features

  • One-component anaerobic system: Requires no mixing and cures when confined in the absence of air between close-fitting metal surfaces.
  • Immediate low-pressure sealing: Properly tightened fittings seal instantly to moderate pressures before full cure.
  • Formulated for inactive metals: Cures without heat or activator on stainless steel and other inactive metal surfaces.

Applications / Suitable for

  • Locking and sealing threaded metal pipes and fittings
  • Instrumentation, pumps, valves, hydraulics and compressors
  • Water, coolant, fuel-oil and low-pressure steam piping
  • Threaded fittings in fossil-fuel, solar and hydro power-plant piping systems
Product Family

LOCTITE 580

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured properties unless identified as LOCTITE Material Specification limits.

Property Value Unit Method / condition
Appearance Smooth, creamy, off-white paste — Uncured; LMS
Specific gravity 1.08 — 25 °C
Viscosity 300,000–900,000 mPa·s (cP) Brookfield RVF, spindle 7, 2 rpm, 25 °C; LMS
Halogen content ≤200 ppm LMS
Chlorine content ≤200 ppm LMS
Sulfur content ≤1,500 ppm LMS
Technical properties

After-processing / final-state properties

Typical cured-material properties and test results. Breakaway-torque values identified as LMS are specification-controlled limits.

Property Value Unit Method / condition
Coefficient of thermal expansion 0.1 K−1 ISO 11359-2
Coefficient of thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Cured material
Breakaway torque ≥0.9 N·m ISO 10964; 3/8 × 24 grade 2 steel nuts and bolts; 24 hours at 25 °C; LMS
Breakaway torque ≥2.3 N·m ISO 10964; 3/8 × 24 grade 2 steel nuts and bolts; cured 24 hours at 93 °C and tested at 25 °C; LMS

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers