LOCTITE SI5092

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI5092

Main features

  • Yellow to Green liquid
  • UV Cure
  • Non corrosive

Product Description

LOCTITE® SI 5092™ is used for potting, coating and sealing of various automotive, electronic, military and industrial components. It is highly flexible and enhances the load bearing and shock absorbing characteristics of the bond area.

LOCTITE® SI 5092™ is a non corrosive, single component alkoxy silicone that requires no mixing and can cure with Ultraviolet light. Moisture is utilized as a secondary cure to cure shadowed areas. This self-leveling product offers uniform cavity fills.

Product Family

221934

300 mL - Cartridge | Green
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 63 days
CA No longer available
EU Shipping in 110 days
Packaging
Unit of measure Cartridge
Net weight 301 g
Gross weight 359 g
Dimensions 5 x 5 x 22.9 cm
TDS, SDS & Technical Documents

Technical Specifications

Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
64000000000000 Ohms⋅cm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
75 %
Chemical Properties
Water Absorption
0.6 %

Additional Information

Typical curing performance

Normal processing conditions will include exposure to sufficient UV light irradiance to effectively cure the material. Surface and/or atmospheric moisture will promote the cure of material in shadowed regions. Although functional strength is developed almost instantly due to the UV curing nature of LOCTITE® SI 5092™, increased cure properties are developed during 72 hours at ambient conditions.

Surface Cure

When curing with sufficient UV light irradiance, exposed material will cure dry to the touch in seconds. Atmospheric moisture cures material not exposed to UV light.

Depth of Cure

Shadowed areas rely on surface and/or atmospheric moisture to effect cure. Depth of cure is limited to approximately 6 millimeters and will take at least 24 hours to develop. Rapid depth of cure can be attained with focused UV light.