PERMATEX FORM-A-GASKET NO. 2

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMATEX 1

Main features

  • Hard-Setting Permanent Gasket Sealing
  • 2-Hour Return to Operation
  • Wide Continuous Temperature Resistance

Product Description

Permatex Form-A-Gasket No. 1 Sealant is a hard-setting, semi-flexible gasket sealant for permanent rigid flanges, threaded connections and gasketed assemblies. The single-part viscous paste cures by solvent evaporation and can be used with new or existing gaskets as well as flange and fitting interfaces. Assemblies are operational after 2 hours, while full cure is effective after 24 hours. The cured sealant has a continuous temperature range of -54 to 204 deg C and retains effective properties in contact with water, ethylene glycol, non-ethanol gasoline, motor oil, transmission fluid and sea water.

Key features

  • Hard-setting solvent-evaporation cure: The viscous paste cures to a hard, semi-flexible seal by solvent evaporation.
  • 2-hour return to operation: Assemblies are operational after 2 hours; full cure is effective after 24 hours.
  • -54 to 204 deg C continuous range: The cured sealant is rated for continuous temperature exposure from -54 to 204 deg C.

Applications

Flanges and new or existing gaskets; threaded and hose connections; cover plates; freeze plugs and manifold gaskets; pipe and plumbing connections; permanent rigid assemblies.

Product Family

PERMATEX 1

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Red - brown paste
Chemistry Type
Modified resin, fillers & alcohol
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.5

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical typeModified resin, fillers and alcohol-Uncured sealant
Physical formViscous paste-Uncured sealant
Specific gravity1.5-Uncured sealant