PLEXUS MA1130

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Plexus® MA1130 | Two-Part Methacrylate Adhesive

Main features

  • Two-part methacrylate for multi-material structural bonding
  • 26–33 minute work time at 75°F
  • Gap tolerance up to 0.5 inch

Product Description

Plexus® MA1130 is a two-part methacrylate structural adhesive for bonding composites and primed metals, with additional use on thermoplastic, metal, and composite assemblies. The 10:1 by-volume system provides a typical 26–33 minute working time at 75°F (23.9°C), 0.03–0.5 in (0.75–12.4 mm) gap tolerance, and a gray cured color. It can be dispensed from ready-to-use cartridges or bulk pails and drums. Limited surface preparation may be sufficient on supported substrates, while PC120 Cleaner Conditioner is recommended on metal.

Key features

  • Multi-material structural bonding: Designed for composites and primed metals, with bonding use across thermoplastic, metal, and composite assemblies.
  • Controlled processing window: 10:1 mix ratio by volume, typical 26–33 minute work time at 75°F (23.9°C), and 0.03–0.5 in (0.75–12.4 mm) gap tolerance.
  • Cured mechanical profile: Typical tensile strength of 2,800–3,200 psi (19.3–22.1 MPa), 30–45% elongation at break, and Shore D 75 hardness.

Applications / Suitable for

  • Structural bonding of composites and primed metals
  • Thermoplastic, metal, and composite assemblies
Product Family

PLEXUS MA1130

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Structural adhesive

Plexus® MA1130

Plexus® MA1130 is a two-part methacrylate structural adhesive for bonding composites and primed metals, with additional use on thermoplastic, metal, and composite assemblies. The 10:1 system combines an extended working window with substantial gap tolerance and cartridge or bulk dispensing options.

Two-part methacrylate 10:1 mix ratio by volume 26–33 min work time at 75°F 0.03–0.5 in gap tolerance Cartridge or bulk dispensing
Technical properties

As-supplied properties

Typical component properties before mixing. Part A / Part B order is preserved where paired.

Property Value Unit Method / condition
Color Off-white / Charcoal – Part A / Part B
Mix ratio by volume 10:1 A:B Part A to Part B
Mix ratio by weight 10.4:1.0 A:B Part A to Part B
Component density 0.98 / 0.95 g/mL Part A / Part B
Component viscosity 110–150 / 90–130 ×10³ cP Part A / Part B
Bonding process

Processing and application

MA1130 can be dispensed from handheld cartridges or automatic meter/mix/dispense equipment. Bonding performance depends on maintaining the specified component ratio, controlling adhesive temperature, preparing contaminated surfaces appropriately, and mating the parts within the working time.

Mix ratio: 10:1 by volume or 10.4:1.0 by weight, Part A to Part B.
Recommended application temperature: 65–85°F (18–30°C). Temperatures outside this range can significantly change the cure rate.
Typical work time: 26–33 minutes at 75°F (23.9°C). Adhesive and activator temperature should be held reasonably constant for consistent dispensing.

Recommended bonding sequence

Stage 1
Prepare the bonding surfaces
Keep surfaces free of grease, dirt, and other contaminants. Plastics, coated metals, and raw metals may require only a dry rag or light solvent depending on surface condition. Dust-free composites may be bonded as-is or lightly abraded to remove mold release or increase surface area. PC120 Cleaner Conditioner is recommended on metal.
Stage 2
Mix and dispense
Load the cartridge and remove the end caps, attach the mixing tip, and dispense a mixer’s length before applying adhesive. Apply enough material to completely fill the joint when parts are mated. Handheld cartridges and automatic meter/mix/dispense equipment are supported.
Stage 3
Mate, fixture, and build strength
Mate parts within the working time and fix them in position until sufficient bond strength is achieved. Typical profiles at 60°F / 75°F / 90°F are: work time 30–40 / 26–33 / 15–20 min; time to 50 psi 45–50 / 35–40 / 25–35 min; time to 500 psi 65–75 / 60–70 / 35–40 min; and time to 1,000 psi >100 / 100–110 / 45–50 min. A post-bake is required for ultimate performance on thin-gauge metals. Contact Krayden for the applicable post-bake schedule.
Storage and Handling

Shelf life is 6 months based on continuous storage between 55°F and 77°F (13°C and 25°C). Intermittent or prolonged exposure above 80°F (27°C) reduces shelf life, and exposure above 100°F (38°C) should be avoided. Cool storage between 45°F and 65°F (7°C and 18°C) may extend shelf life; return cold-stored material to room temperature before use. Mixing large masses can generate substantial exothermic heat, so dispense only the quantity that can be used within the working time and keep gap thickness within the product’s maximum gap-fill capability.

Cured performance

Typical cured properties

Typical cured material properties. Tensile properties are in accordance with ASTM D638 / ISO 527.

Property Value Unit Method / condition
Final color Gray – Cured adhesive
Gap tolerance 0.03–0.5 in 0.75–12.4 mm; gap tolerance, not a universal recommended bondline thickness
Hardness 75 Shore D Typical cured property
Tensile strength 2,800–3,200 psi 19.3–22.1 MPa; ASTM D638 / ISO 527
Tensile modulus 95–110 kpsi 655–758 MPa; ASTM D638 / ISO 527
Elongation at break 30–45 % ASTM D638 / ISO 527
Peak exotherm time 60–80 min 10 g sample
Peak exotherm temperature 260 (127) °F (°C) 10 g sample
Bond strength

Typical lap shear performance

Typical lap shear values measured according to ASTM D1002. CF indicates cohesive failure. PC120 Cleaner Conditioner is recommended on metal.

Property Value Unit Method / condition
Lap shear, aluminum 2,350 (16.2) psi (MPa) ASTM D1002; cohesive failure
Lap shear, primed steel 2,716 (18.7) psi (MPa) ASTM D1002; cohesive failure

Technical guidance

Bulk dispensing hardware
For pail or drum dispensing, bulk equipment must be explosion proof. Parts in direct contact with the liquid adhesive and activator should be stainless steel. Avoid brass, carbon steel, copper, and copper-containing alloys. Teflon, Teflon-coated PVC foam, ethylene/propylene, or polyethylene are recommended for seals and gaskets; avoid Viton, BUNA-N, Neoprene, and other elastomers.
Clean-up and chemical exposure
Clean-up is easiest before cure using common laboratory solvents, citrus terpene or NMP-containing cleaners, degreasers, or soap and water. Cured adhesive may require careful scraping followed by a cleaning agent. Chemical resistance is described as excellent to hydrocarbons, acids and bases from pH 3–10, and salt solutions, while strong polar solvents and strong acids or bases are identified as susceptibility areas. Actual resistance depends on contact mode, frequency, duration, and temperature.
Next steps

Evaluate Plexus® MA1130 for your assembly

Need to validate MA1130 for a specific substrate pair, bond gap, dispense method, or temperature profile? Krayden can help review joint requirements, surface preparation, processing conditions, and the product’s typical strength data before application testing.