PLEXUS MA422

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ITW PLEXUS MA422

Main features

  • 10:1 Controlled Mixing
  • 17 to 20-Minute Working Window
  • 0.75 to 9.5 mm Gap Range

Product Description

PLEXUS® MA422 Methacrylate Adhesive is a two-part, 10:1 methacrylate structural adhesive for bonding composite, thermoplastic, and metal assemblies. The blue, non-sag mixed system provides a typical 17 to 20 minute working time at 23°C and reaches approximately 75% of ultimate strength in 35 to 40 minutes under the documented conditions. It supports bondline gaps from 0.75 to 9.5 mm and is documented for transportation, marine, and industrial assembly applications where a controlled work window and gap-filling bond are required.

Key features

  • 17 to 20-minute working time: The documented process window is measured at 23°C.
  • Gap-filling structural bond: The adhesive supports documented bondline gaps from 0.75 to 9.5 mm.
  • Ductile cured properties: Typical tensile strength is 16.8 to 20.5 MPa with 40 to 70% elongation.

Applications / Suitable for

  • Transportation assemblies
  • Marine composite bonding
  • Industrial metal, thermoplastic, and composite bonding

Technical Specifications

General Properties
Color
The color
Off-White / Blue
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (A / B)
Density (g)
0.96 / 1.06 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
9:1
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
40 - 70 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color, Part A Off-white N/A As supplied
Color, Part B Blue N/A As supplied
Mix ratio 10:1 parts by volume Part A : Part B
Mix ratio 9:1 parts by weight Part A : Part B
Density, Part A 0.96 g/mL As supplied
Density, Part B 1.06 g/mL As supplied
Viscosity, Part A 100,000 to 130,000 cP As supplied
Working time 17 to 20 min At 23°C
Technical properties

After-processing / final-state properties

Typical final-state values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Recommended bondline gap 0.75 to 9.5 mm Documented range
Hardness 70 Shore D Typical cured value
Tensile strength 16.8 to 20.5 MPa ASTM D638 / ISO 527
Tensile modulus 762 to 1,031 MPa Typical cured value
Elongation 40 to 70 % Typical cured value