PLEXUS MA832

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ITW PLEXUS MA832

Main features

  • 10:1 Controlled Mixing
  • 12 to 14-Minute Working Window
  • Glass-Bead Bondline Control

Product Description

PLEXUS® MA832 Methacrylate Adhesive is a two-part, 10:1 methacrylate structural adhesive for bonding many metals without primer and for selected thermoplastic and composite assemblies. The gray, non-sag mixed adhesive includes glass beads for bondline control and provides a typical 12 to 14 minute working time. Under the documented conditions, it develops 500 psi handling strength in approximately 65 to 70 minutes. The system supports bondline gaps from 0.25 to 13 mm and develops Shore D 71 hardness after cure.

Key features

  • Primerless metal bonding: The adhesive is documented for structural bonding to many metal substrates without a separate primer.
  • 12 to 14-minute working time: The system reaches 500 psi handling strength in approximately 65 to 70 minutes.
  • Wide bondline range: Documented gap capability is 0.25 to 13 mm with glass beads for bondline control.

Applications / Suitable for

  • Structural bonding of metal assemblies
  • Selected thermoplastic assemblies
  • Composite assembly bonding

Technical Specifications

General Properties
Color
The color
Off-White / Grey or Grey GB
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Adhesive / Activator)
Density (g)
0.97 / 1.09 or 1.11 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
8.86 / 1.0 or 1.02
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
11 °C
Operating Temperature
-40– 82 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color, Part A Off-white N/A As supplied
Color, Part B Gray or gray with glass beads N/A As supplied
Mix ratio 10:1 parts by volume Part A : Part B
Mix ratio 8.86:1 parts by weight Part A : Part B
Density, Part A 0.97 g/mL As supplied
Density, Part B 1.11 g/mL As supplied
Viscosity, Part A 80,000 to 130,000 cP As supplied
Working time 12 to 14 min Documented application condition
Technical properties

After-processing / final-state properties

Typical final-state values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Recommended bondline gap 0.75 to 9.5 mm Documented range
Hardness 70 Shore D Typical cured value
Tensile strength 16.8 to 20.5 MPa ASTM D638 / ISO 527
Tensile modulus 762 to 1,031 MPa Typical cured value
Elongation 40 to 70 % Typical cured value

Leading Brands Trust in Our Products and Services