SOLSTICE PTM7000
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 0.06 Thermal Impedance
- 6.5 Thermal Conductivity
- Pad form
Product Description
PTM7000 is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. As with all Phase change materials, it has stable Thermal Impedance across accelerated aging tests and does not display bleed, pump or flow out. PTM7XXX product line has the highest Thermal conductivity and lowest thermal impedance out of the entire PTM Series.
PTM7000 has a Thermal conductivity of 6.5 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. Typical temperature range is -40°C to 125°C. This proprietary material provides superior reliability and maintains low thermal impedance (0.06) , making it desirable for high-performance integrated circuit devices. Regarding breakdown voltage, phase change materials are typically aroun 5000V/mm but this is highly thickness depend. Naturally an initial "unphased" 0.2mm pad will have different BV than the final 30/40um bondline.
Please keep in mind that 7XXX is a Product Series. Base 7000 performs on the baseline of the stated properties while PTM7900 and PTM7950 are the highest performing materials of this product line reaching 8.5 W/m·K and 0.04 TI.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
Phase Change Activation and Bond Line Thickness Reduction
Solstice PTM7000 upon reaching its phase change temperature, the material softens and becomes more conformable, allowing it to flow under applied pressure and accommodate surface irregularities between mating interfaces.
This phase change behavior enables PTM7000 to progressively reduce its bond line thickness (BLT), minimizing the thickness of the thermal interface and potentially reducing the thermal resistance between contacting surfaces.
Temperature-Dependent Thin-Down Behavior
The PTM7000 thin-down curves demonstrate the influence of temperature on material flow and thickness reduction during thermal activation.
At elevated temperatures of 50°C, 65°C, and 80°C, PTM7000 exhibits progressive thickness reduction, with higher temperatures producing faster initial thin-down rates.
These results demonstrate how increasing the activation temperature can accelerate material conformability and bond line thickness reduction.
What are the reliability expectations of the PTM 7XXX products?
All the 7XXXseries (7000, 7900 & 7950) pass the three major reliability tests with flying colours. Honeywell does not test beyond 1000 cycles, 92 hrs HAST and 1000 hrs HTS. However, anecdotally, some automotive customers have taken 7900 to beyond Honeywell’s limits and have found it to pass shock and vibration, longer temperature cycling and longer temperature and humidity soak.

PTM7XXX Series - Pressure vs Thermal Impedance
PTM7XXX Series vs Competition comparison
Case Study: Dripping Test for PTM 7000 on Power Device
| Product | Unit | ANTI - DRIPPING RESULT (TEMPERATURE CYCLE) | |
| 400X | 800X | ||
| PTM7000 - Pad | No shim | Pass | Pass |
PTM7000 passed the dripping test up to 800x cycle with a power device
Case Study: PTM 7000 Thermal Cycling Aging & High Temperature Baking up to 2000 hours