STYCAST US 2350
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Flame retardent
- Low CTE
- Room temperature curing
Product Description
LOCTITE STYCAST US 2350 is a flexible, flame retardant, mineral-filled, polyurethane compound. This potting compound has long pot life, and is low viscosity so it flows well and adheres to many substrates. It has very low odor and does not contain TDI or mercury compounds.
LOCTITE STYCAST US 2350 has a mixing ratio 1:4 by volume and cures at room temperature.
Packaging
Unit of measure Cartridge
Net weight 670 g
Gross weight 842 g
Dimensions 9.1 x 6 x 22.9 cm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)
1.4 g/cm3
Mix Ratio
21.2:100
The amount of a constituent divided by the total amount of all other constituents in a mixture
Work life @25°C
0.75 hours
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate.
It is based on the change in viscosity and it can rely on the application requirements.
Thermal Properties
UL 94 Rating
V2
Flammability rating classification.
It determines how fast a material burns or extinguishes once it is ignited.
HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm
V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed.
V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed.
V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed.
5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole.
5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
Electrical Properties
Surface Resistivity
1540000000000000 Ohms/sq
Volume Resistivity
61200000000000 Ohms⋅cm
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
Chemical Properties
Water Absorption
0.09 %
Additional Information
Recommended Curing Conditions
- 12 to 24 hours @ 23 °C
Alternate Cure Schedule
- 1 to 3 hours @ 65 to 85°C