Protect Electronics in Harsh Conditions

Flight-Ready Encapsulation and Coatings

Aerospace & Defense Electronics Protection

 Aircraft cockpit showing avionics instruments, navigation displays, and electronic controls

Aerospace and defense electronic assemblies used in avionics, sensing, communication, navigation, control, mission, and power systems must maintain reliable performance under demanding mechanical, thermal, electrical, and environmental conditions.

Temperature cycling, vibration and shock, moisture, contamination, corrosion, and heat generation can affect components, solder joints, interconnections, and printed circuit board assemblies.

Krayden supports material technologies that protect aerospace and defense electronics at the component, PCB, module, and enclosure level.

Protection Technologies

Protecting Aerospace & Defense Electronics in Harsh Operating Environments

The following operating conditions represent key challenges for aerospace and defense electronics, along with their potential effects and the material protection approaches commonly evaluated for each.

Thermal Stress & Thermal Cycling +
Aerospace electronic assembly exposed to changing operating temperatures

Avionics modules, radar and sensor electronics, power electronics, and other aerospace assemblies can experience repeated temperature changes during operation, altitude transitions, and mission cycles. Components, solder joints, printed circuit boards, adhesives, encapsulants, and housings can expand and contract at different rates, concentrating stress at package interfaces and electrical interconnections.

Primary Stressors

Temperature extremes, repeated thermal cycling, and thermal-expansion differences between components, PCBs, solder joints, housings, and protective materials.

Potential Effects

Solder-joint fatigue, package stress, cracking, delamination, loss of adhesion, and mechanical stress on sensitive electronic components.

Relevant Protection Approaches

Underfill, compliant encapsulation, flexible bonding materials, and thermal management materials selected for the assembly's operating environment.

Vibration & Mechanical Shock +
Aerospace electronic assembly exposed to vibration and mechanical shock

Aerospace electronics can be exposed to continuous vibration, mechanical shock, and transient loading generated during aircraft operation, propulsion, maneuvering, launch, landing, or other mission conditions. Larger PCB components, connectors, leads, solder joints, and bonded interfaces may require additional mechanical reinforcement to limit movement and maintain reliable electrical connections.

Primary Stressors

Aircraft and platform vibration, mechanical shock, PCB flexing, inertial loading, and movement of larger or heavier electronic components.

Potential Effects

Component movement, solder-joint fatigue, cracked connections, lead or connector movement, and failure at bonded or mechanically loaded interfaces.

Relevant Protection Approaches

Component staking, underfill, flexible bonding, and localized or full encapsulation where additional mechanical reinforcement is required.

Moisture, Contamination & Corrosion +
Aerospace electronics protected against moisture contamination and corrosion

Aerospace and defense electronic assemblies may encounter humidity, condensation, airborne contaminants, ionic residues, corrosive environments, and service-related chemical exposure. These conditions can affect PCB conductors, component leads, solder joints, connectors, and insulating surfaces, increasing the need for controlled environmental protection.

Primary Stressors

Humidity, condensation, ionic contamination, corrosive environments, airborne contaminants, and application-specific chemical exposure.

Potential Effects

Corrosion, leakage current, insulation degradation, electrochemical migration, connector degradation, and reduced long-term electrical reliability.

Relevant Protection Approaches

Conformal coatings, encapsulation and potting, dielectric gels, localized sealing, and electrically insulating protective materials.

Heat Dissipation +
Thermal management in aerospace and defense electronic assemblies

High-density avionics, radar, sensing, communication, mission-computing, and power-electronics assemblies can generate significant heat within compact electronic modules. Thermal management materials help create controlled heat-transfer paths from components and PCBs to heat spreaders, housings, chassis, or heat sinks while maintaining the electrical and mechanical requirements of the assembly.

Primary Stressors

High power density, compact packaging, limited airflow, localized heat generation, and thermal resistance between components and electronic housings.

Potential Effects

Elevated component temperatures, accelerated material degradation, thermal stress, reduced electrical performance, and shortened electronic service life.

Relevant Protection Approaches

Thermally conductive adhesives, gap fillers, thermal interface materials, and thermally conductive encapsulants selected for the required heat-transfer path.

 Low Pressure, Vacuum & Outgassing +
Aerospace or space electronic assembly where low outgassing may be required

Selected aerospace electronics, particularly space, high-altitude, optical, and high-vacuum assemblies, may require additional control of material volatility and outgassing. Adhesives, encapsulants, coatings, and sealants used around sensitive electronics may therefore require application-specific evaluation for volatile release and contamination behavior. These requirements do not apply equally to every aircraft or avionics system.

Primary Stressors

Reduced atmospheric pressure, vacuum exposure, volatile material release, and contamination-sensitive electronic or optical assemblies.

Potential Effects

Outgassing, contamination of sensitive surfaces, changes in material behavior, and reliability concerns in vacuum or contamination-sensitive environments.

Relevant Protection Approaches

Low-outgassing encapsulants, controlled-volatility sealants, qualified bonding materials, and program-specific material screening.

Material Technologies for Aerospace & Defense Electronics Protection

Aerospace and defense electronics rarely rely on a single protection method. A typical assembly may combine conformal coatings for PCB protection, underfill for solder-joint reinforcement, staking for larger components, thermally conductive materials for heat transfer, and sealants around enclosure and connector interfaces.

The right combination depends on the assembly’s operating environment, exposure to vibration and thermal cycling, electrical insulation requirements, heat generation, rework needs, and any program-specific material constraints.

Conformal coating material for aerospace electronic assemblies
PCB Environmental Protection

Conformal Coatings

Conformal coatings are used on populated circuit boards to provide thin, lightweight protection against moisture, condensation, contamination, corrosion, and electrical leakage. They are especially useful in aerospace electronic assemblies where environmental protection is needed without fully encapsulating the board or adding significant mass.

Typical Materials

Acrylic, urethane, silicone, UV-curable, and dual-cure coating systems.

Aerospace Function

Protects conductors, solder joints, component leads, and insulating surfaces while allowing connectors, test points, and rework areas to remain selectively uncoated.

Selection Focus

Coating thickness, cure mechanism, shadow-area cure, flexibility, temperature cycling, chemical exposure, inspection method, masking requirements, and reworkability.

Where Used: Avionics PCBs  •  Radar & Sensor Electronics  •  Communication & Navigation Assemblies

Encapsulation and potting material for aerospace electronic assemblies
Environmental & Electrical Protection

Encapsulation & Potting

Encapsulation and potting materials surround components or complete assemblies to provide broader protection than conformal coatings. In aerospace electronics, they are often used where assemblies require stronger resistance to moisture, contamination, electrical stress, vibration, and shock, or where added dielectric or thermal performance is needed.

Typical Materials

Epoxy encapsulants, silicone elastomers, polyurethane systems, dielectric gels, and thermally conductive potting compounds.

Aerospace Function

Provides broader environmental and dielectric protection while helping support components against vibration, shock, and handling stresses.

Selection Focus

Modulus, thermal expansion, dielectric properties, thermal conductivity, cure exotherm, weight, operating temperature, and stress on sensitive components.

Where Used: Avionics Modules  •  Sensors & Connectors  •  Power Electronics

Underfill material for aerospace electronic assemblies
Solder Joint Reinforcement

Underfill

Underfill materials are used beneath surface-mounted packages to reinforce solder interconnections and reduce localized stress. In aerospace electronics, they are especially relevant for assemblies exposed to vibration, thermal cycling, and board flexing, where solder-joint reliability is a key concern.

Typical Materials

Capillary-flow epoxy underfills, reworkable underfills, and specialized low-outgassing underfill systems.

Aerospace Function

Helps redistribute stress away from solder joints and into the package-to-board interface, improving resistance to vibration and repeated thermal expansion mismatch.

Selection Focus

Package geometry, flow behavior, cure temperature, glass transition temperature, modulus, thermal expansion, reworkability, and thermal cycling performance.

Where Used: BGA Packages  •  High-Density PCBs  •  Mission & Sensor Electronics

Component staking and bonding material for aerospace electronic assemblies
Vibration & Mechanical Reinforcement

Component Staking & Bonding

Staking and electronic bonding materials help secure larger, taller, or mechanically sensitive components that could otherwise shift under vibration, shock, or repeated loading. In aerospace systems, they are used to reduce stress on leads, solder joints, and connectors and to improve the mechanical stability of the assembly.

Typical Materials

Non-sag epoxy staking compounds, flexible epoxy adhesives, urethane adhesives, and electrically insulating electronic bonding materials.

Aerospace Function

Restrains component movement and transfers mechanical load into the board or adjacent attachment area, reducing repeated loading on leads, solder joints, and connectors.

Selection Focus

Component mass and height, vibration spectrum, shock loading, adhesive flexibility, non-sag behavior, bond geometry, electrical insulation, cure temperature, and repair access.

Where Used: Large Components  •  Connectors  •  Vibration-Sensitive PCBs

Thermal management material for aerospace electronic assemblies
Heat Transfer & Temperature Control

Thermal Management Materials

Thermal management materials help move heat away from electronic components and into housings, chassis, heat spreaders, or heat sinks. In aerospace electronics, they are important in compact or high-power assemblies where excess heat can affect reliability, performance, and long-term service life.

Typical Materials

Thermally conductive adhesives, gap fillers, thermal tapes, pads, interface materials, and thermally conductive encapsulants.

Aerospace Function

Improves heat dissipation by creating controlled thermal paths across gaps and interfaces while supporting the electrical and mechanical needs of the assembly.

Selection Focus

Thermal conductivity, interface thickness, dielectric performance, compressibility, adhesion, operating temperature, vibration resistance, and thermal cycling.

Where Used: PCB-to-Housing Interfaces  •  Power Devices  •  High-Power Modules

Electronic sealing material for aerospace electronic assemblies
Localized Environmental Sealing

Electronic Sealants

Electronic sealants help protect critical interfaces where moisture, contaminants, or other environmental exposure could enter an assembly. In aerospace electronics, they are commonly considered around housings, connectors, cable entries, sensors, and other localized sealing points where flexibility and electrical insulation may be important.

Typical Materials

RTV silicone sealants, controlled-volatility silicones, low-outgassing sealants, and flexible electrically insulating sealing materials.

Aerospace Function

Seals joints and interfaces to help block moisture and contamination while accommodating differential movement, vibration, and thermal expansion.

Selection Focus

Flexibility, elongation, adhesion, dielectric properties, cure chemistry, temperature range, moisture resistance, and low-outgassing requirements where applicable.

Where Used: Housings & Enclosures  •  Connectors & Cable Entries  •  Sensors & Optical Assemblies

Featured Materials

Aerospace Electronics Protection Materials

Krayden supplies materials from Dow / DOWSIL, HumiSeal, Henkel / LOCTITE, and 3M for aerospace and defense electronic assemblies. These materials support conformal coating, encapsulation, underfill, component staking, thermal management, flexible bonding, electrical insulation, and sealing across PCB, module, sensor, power-electronics, and enclosure applications.

Dow DOWSIL
Dow Aerospace Electronics Materials

Silicone Protection & Thermal Management for Aerospace and Defense Electronics

DOWSIL materials help aerospace and space electronics manage heat, electrical insulation, environmental exposure, mechanical stress, and material volatility. The products below cover encapsulation, conformal coating, thermal gap filling, thermally conductive bonding, and sealing, including options for low-outgassing and vacuum-sensitive electronic assemblies.

DOWSIL 93-500 Space Grade Encapsulant
Space-Grade Encapsulation

DOWSIL 93-500

Transparent, flowable, two-part addition-cure silicone elastomer for encapsulating, potting, bonding, sealing, and coating electronic and optical assemblies used in terrestrial and space systems.

  • 10:1 mix ratio by weight with a typical 2.5-hour pot life
  • Operating range from -115°C to 200°C after cure
  • 18 kV/mm dielectric strength and 170% typical elongation
★ Typical thermal-vacuum weight loss: 0.20%; volatile condensable material: 0.01%
DOWSIL EA-9187L silicone conformal coating
One-Part Silicone Conformal Coating

DOWSIL EA-9187L

One-part, translucent, no-added-solvent silicone conformal coating for protecting printed circuit board assemblies and sensitive electronic components. After cure, it forms a soft, stress-relieving electrically insulating elastomer.

  • Typical viscosity of 900 mPa·s for spray or dip application
  • Typical Shore A 17 hardness and 165% elongation after cure
  • UV indicator for inspection with UL 94 V-0 and UL 746C recognition
★ 20 kV/mm typical dielectric strength after cure
DOWSIL TC-6040 Thermal Conductive Encapsulant
Thermally Conductive Encapsulation

DOWSIL TC-6040

Two-part, flowable thermally conductive silicone encapsulant for electronic assemblies that need component protection, stress relief, and a path for transferring heat away from heat-generating areas.

  • 4.0 W/m·K thermal conductivity
  • 24-hour cure at 25°C or 60-minute cure at 100°C
  • 32 Shore A hardness with high-temperature stability up to 175°C
★ Meets ASTM E595 outgassing requirements
DOWSIL TC-5533 Gap Filler
Thermal Gap Filling

DOWSIL TC-5533

Two-part, low-density thermally conductive gap filler for filling uneven interfaces between electronic components and housings, chassis, or heat spreaders while supporting heat dissipation, vibration damping, and stress relief.

  • 3.0 W/m·K thermal conductivity
  • 24-hour cure at 25°C or 1-hour cure at 125°C
  • 65 Shore 00 hardness with controlled siloxane volatility below 100 ppm
★ Meets ASTM E595 outgassing requirements
DOWSIL TC-2035 CV Adhesive
Thermally Conductive Adhesive

DOWSIL TC-2035 CV

Two-part thermally conductive silicone adhesive for bonding electronic components while creating a heat-transfer path to heat sinks, housings, and other thermal-management structures.

  • 3.3 W/m·K thermal conductivity
  • 15-minute heat cure at 115°C
  • 2.9 MPa aluminum lap-shear adhesion with approximately 50% elongation
★ Meets ASTM E595 outgassing requirements
DOWSIL 6-1104 CV Sealant
Controlled-Volatility Sealing

DOWSIL 6-1104 CV

One-part, nonflow, translucent moisture-cure RTV silicone for sealing and bonding space hardware and other sensitive electronics where flexibility, electrical insulation, and low material volatility are important.

  • 610% typical elongation for compliant sealing and stress relief
  • 550 V/mil dielectric strength
  • 41 Shore A hardness and 925 psi tensile strength
★ Extremely low volatility for use in high-vacuum environments
HumiSeal
HumiSeal Aerospace Electronics Materials

Conformal Coatings for Aerospace PCB Environmental Protection

HumiSeal conformal coatings help protect avionics and other aerospace printed circuit assemblies from moisture, contamination, corrosion, and electrical leakage while adding minimal material around the board. UV40 supports fast UV processing with secondary moisture cure in shadowed areas, while 1B73 provides a fast-drying acrylic coating that supports inspection, repair, and long-term electrical protection.

HumiSeal UV40 conformal coating
UV / Secondary-Cure Conformal Coating

HumiSeal UV40

Single-component, high-solids, UV-curable acrylated polyurethane conformal coating combining rapid UV processing with secondary moisture cure of unexposed areas. It also fluoresces under UV light to support coating inspection.

  • Minimum 95% solids content
  • Recommended coating thickness of 25 to 125 microns
  • Secondary moisture cure reaches shadowed areas within 2 to 3 days at ambient conditions
  • MIL-I-46058C qualified and IPC-CC-830 compliant
HumiSeal 1B73 acrylic conformal coating
Acrylic Conformal Coating

HumiSeal 1B73

Single-component, fast-drying acrylic conformal coating for printed circuit assemblies. The cured coating provides flexibility and electrical protection, fluoresces under UV light for inspection, and can be repaired when required.

  • Typical 30-minute drying time to handle
  • Recommended coating thickness of 25 to 75 microns
  • 6,300 V dielectric breakdown voltage with thermal-shock data from -65°C to 125°C
  • MIL-I-46058C qualified, IPC-CC-830 compliant, and UL recognized
Henkel LOCTITE
Henkel LOCTITE Electronic Materials

Component Reinforcement, Underfill & Encapsulation

LOCTITE electronic materials help protect aerospace electronics at the component and package level. ABLESTIK 2112 stabilizes and reinforces PCB components, ECCOBOND UF1173 supports BGA and CSP solder joints during thermal and mechanical loading, and STYCAST 2850FT provides electrically insulating encapsulation where heat dissipation and mechanical protection are both required.

LOCTITE ABLESTIK 2112
Component Staking

LOCTITE ABLESTIK 2112

Two-component, thixotropic, non-conductive epoxy adhesive for critical electronic and aerospace bonding, laminating, reinforcing, and PCB component staking. Its non-sag rheology supports controlled placement around components.

  • 100:22 resin-to-hardener mix ratio by weight
  • 60,000 mPa·s mixed viscosity with thixotropic, non-sag behavior
  • Typical 30-minute pot life at 25°C
  • -60°C to 125°C service range with 410 V/mil dielectric strength
LOCTITE ECCOBOND UF1173 underfill
Board-Level Underfill

LOCTITE ECCOBOND UF1173

One-component, low-CTE underfill formulated to flow beneath CSP and BGA packages and distribute mechanical stress away from solder interconnections, helping improve solder-joint reliability during temperature cycling and mechanical loading.

  • 5-minute cure at 150°C
  • 160°C glass transition temperature
  • 7,500 mPa·s viscosity for jet or needle dispensing
  • 0.55 W/m·K thermal conductivity
LOCTITE STYCAST 2850FT thermally conductive encapsulant
Thermally Conductive Encapsulation

LOCTITE STYCAST 2850FT

Thermally conductive, electrically insulating epoxy encapsulant for electronic components that need heat dissipation together with thermal-shock and mechanical protection. Final properties depend on the catalyst system selected for processing and performance requirements.

  • With CAT 9: 1.25 W/m·K thermal conductivity and 86°C glass transition temperature
  • With CAT 9: 14.4 kV/mm dielectric strength
  • Typical 0.03% water absorption with CAT 9
  • TML 0.25% and CVCM 0.01% per NASA Reference Publication 1124 for the stated cure condition
3M
3M Electronic Materials

Electrical Protection, Flexible Bonding & Thermal Interfaces

3M materials support aerospace electronic assemblies where electrical insulation, environmental protection, movement, vibration, and heat transfer must be managed. Scotchcast Electrical Resin 281 protects and insulates electrical and electronic components, Scotch-Weld 2216NS provides flexible bonding for assemblies exposed to movement and temperature change, and 8805 creates a thin adhesive thermal path from heat-generating components to cooling structures.

3M Scotchcast Electrical Resin 281
Electrical & Electronic Encapsulation

3M Scotchcast Electrical Resin 281

Two-part, oven-curing filled epoxy resin for electrical and electronic components requiring insulation and protective encapsulation. The cured material is semi-flexible and provides resistance to moisture, chemicals, thermal shock, and mechanical shock.

  • 22-minute gel time at 121°C
  • 65 Shore D hardness
  • Class F temperature rating of 155°C
  • 45% elongation with chemical- and moisture-resistant cured properties
3M Scotch-Weld Epoxy Adhesive 2216NS
Flexible Bonding

3M Scotch-Weld 2216NS

Non-sag, flexible epoxy adhesive for bonded assemblies that need to accommodate expansion, contraction, limited movement, and differences in substrate thermal expansion while maintaining bond strength.

  • Up to 120 minutes of working time
  • Can reach full cure in 30 minutes at 93°C
  • Bonded shear strength up to 3,200 psi at 24°C
  • Cryogenic bonding capability at temperatures down to -252°C
3M Thermally Conductive Adhesive Transfer Tape 8805
Thermally conductive tape

3M 8805

Thermally conductive adhesive transfer tape for creating a thin heat-transfer path between heat-generating electronic components and heat sinks, spreaders, heat pipes, fans, or other cooling structures.

  • Good thermal transfer in a thin adhesive interface
  • High mechanical strength with excellent shock performance
  • Improved wet-out on rough and low-surface-energy substrates
  • Soft, conformable construction supports contact with non-flat surfaces
Related Blogs

Further Reading on Aerospace Electronics Protection Solutions

Common conformal coating defects and prevention methods
Conformal Coatings

Common Conformal Coating Defects and How to Prevent Them

Alicia Montesclaros  •  April 2026

The blog explains common conformal coating defects such as dewetting, bubbles, and delamination, and outlines how cleaning, application control, and process optimization can help prevent them and support long-term PCB reliability.

Thermally conductive potting materials for high-power electronics
Encapsulation & Thermal Management

How Potting Materials Improve Heat Flow and Reliability in High-Power Electronics

James Baduria  •  January 2026

The blog explains how thermally conductive potting materials support heat dissipation, electrical insulation, and environmental protection in high-power electronics while helping reduce thermal stress and related reliability risks.

Conformal coating protection against sulfur corrosion in electronics
Corrosion Protection

Protecting Electronics Against Sulfur Corrosion Using Conformal Coatings

Alicia Montesclaros  •  February 2026

The blog explains how sulfur-containing gases can corrode sensitive electronic components and how coating selection, material properties, and application strategy can help limit sulfur ingress in harsh operating environments.

FAQ

Frequently Asked Questions About Aerospace Electronics Protection

Do conformal coatings make electronics waterproof? +

Conformal coatings help protect printed circuit assemblies from humidity, condensation, contamination, and limited moisture exposure, but they do not automatically make an electronic assembly waterproof. Applications requiring a higher level of environmental isolation may also use encapsulation, potting, enclosure sealing, or a combination of protection methods depending on the assembly design and operating environment.

How do I choose the right protection method for an aerospace PCB assembly? +

Material selection depends on the operating environment, vibration and shock exposure, temperature range and cycling, moisture or contamination risk, electrical insulation requirements, heat generation, component geometry, and serviceability needs. Conformal coatings provide lightweight board-level protection, underfills reinforce package-to-PCB interfaces, staking materials stabilize larger components, thermal materials support heat transfer, and encapsulation or sealing can provide more localized or extensive environmental protection.

Can multiple protection materials be used in a single electronic assembly? +

Yes. Aerospace and defense electronic assemblies often use different materials at different protection levels. An assembly may use underfill beneath BGA or CSP packages, staking around larger components, conformal coating across exposed PCB areas, thermal interface materials between heat-generating components and a housing, and sealants around enclosure or connector interfaces.

When should encapsulation or full potting be considered? +

Encapsulation or full potting may be considered when an electronic assembly requires more extensive environmental, dielectric, mechanical, or thermal protection than a thin conformal coating can provide. Selection should account for material modulus, thermal expansion, cure exotherm, dielectric performance, thermal conductivity, added weight, component stress, repairability, and any applicable aerospace or defense program requirements.

Need Help Selecting Materials for Aerospace Electronics Protection?

Material selection depends on the assembly design, operating environment, vibration and shock exposure, temperature range and cycling, moisture or contamination risk, heat generation, electrical requirements, manufacturing process, and applicable aerospace or defense program requirements. Krayden can support material selection, technical data review, and application guidance across conformal coatings, encapsulants, underfills, staking materials, thermal-management materials, and electronic sealants.

Aerospace Electronics Protection – Quick Reference

PCB Environmental Protection Conformal Coatings
Solder-Joint & Component Reinforcement Underfill & Component Staking
Module & Assembly Protection Encapsulation & Potting
Heat Transfer & Temperature Control Thermal Management Materials
Housing, Connector & Interface Protection Electronic Sealants

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers