In100 | Pure Indium Solder Spheres

Harmonization Code : 8112.99.00 | Other base metals: Gallium, Indium, Vanadium

In100 Pure Indium Solder Spheres Periodic Table In100 Pure Indium Solder Spheres

Main features

  • 100% Pure Indium Solder Spheres
  • Soldering to non-metals
  • Low Eutectic Melting temperature

Product Description

LINQALLOY In100 Pure Indium Solder Spheres are a unique class of solder balls. This alloy is unique in that it alloys you to solder to non-metals, such as glass, quartz or ceramic. This is particularly useful in applications such as battery manufacturing and others where the two parts in questions are not of the same metal type, or not even made of metal at all. The alloy, as the name implies is 99.99% pure indium and as such is written simply as In100.

Features:

  • Solder Balls are made using 100% pure Indium
  • Low-Eutectic melting temperature of 156.6°C
  • Allows soldering to non-metals such as glass, quartz and ceramic

Furthermore, each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the In100 solder balls meet the following quality criteria:

  • Indium (In): 100%
  • Melting Temperature (Eutectic): 156.6°C
  • Sphericity: Within 1.5%

Diameter Tolerance

  • 0.1mm - 0.25mm (100µm - 250µm) : ± 0.0050mm (± 5µm)
  • 0.3mm - 0.45mm (300µm - 450µm) : ± 0.010mm (± 10µm)
  • 0.5mm - 0.89mm (500µm - 890µm) :  ± 0.020mm ( ± 20µm)
Product Family

233249

Alloy: In100 » 0.300mm (12mil) » 10g per jar
1. Select Diameter
2. Select Package Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Unit of measure Jar
Net weight 0.1322 kg
Gross weight 0.1322 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
In100
Alloy Type
A metallic element type
Indium
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
7.31
Spheroid Tolerance
The allowed % that a solder ball (solder sphere) can divert from being perfectly round and spherical. We take one lot of solder spheres and divide it into 4 smaller lots. Each lot is then checked with advanced visual inspection systems. If even 1 ball is out of spec, the entire batch is scrapped and reworked!
1.5 %
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes

Additional Information

What do I get when I buy IN100 Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

Furthermore, each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the In100 solder balls meet the following quality criteria:

  • Indium (In): 100%
  • Melting Temperature (Eutectic): 156.6°C
  • Spheroid Tolerance : Within 1.5%


Presentation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers