Specialty Sealants

Specialized Formulations

Specialty Sealants

Specialty sealants cover chemistries built for demanding sealing applications that fall outside general-purpose epoxy, silicone, and polyurethane systems. This category currently centers on polysulfide sealants, high-performance elastomeric polymers used across aerospace, transportation, marine, and industrial environments, and will expand to include additional specialty chemistries over time.

Polysulfide sealants cure into durable, flexible rubber-like materials. Unlike rigid structural adhesives that transfer mechanical loads, they're designed to accommodate joint movement while maintaining long-term resistance to aviation fuels, hydraulic fluids, chemicals, moisture, UV exposure, and weathering. Their molecular backbone delivers durability without sacrificing elasticity, making them well suited to applications subject to vibration, thermal expansion, and pressure cycling.

From aircraft fuel tank sealing and fuselage assembly to structural glazing, expansion joints, and marine structures, polysulfide sealants provide environmental protection where long service life and chemical resistance are critical. Available in pourable, brushable, and non-sag formulations, they offer strong adhesion to metals, glass, composites, concrete, and many engineering substrates while maintaining a watertight, chemically resistant seal.

While polysulfide sealants provide strong adhesion and long-term environmental sealing, they are primarily designed to seal joints rather than carry structural loads. For high-strength permanent bonding of metals, composites, and engineering plastics, explore the dedicated Structural Epoxy Adhesives category.

46 products

  • P/S 870® Class B Corrosion Inhibitive Sealant

    PPG PS 870

    • Corrosion-Resistant Joint Sealing
    • Long-Term Harsh-Environment Durability
    • Multi-Substrate Aerospace Sealing
  • Teroson AL 6302 Heat Curing Sealant
  • BOSTIK 70-01A

    BOSTIK 70-01A

    • Permanently Elastic SMP Sealant with Temperature Resistance
    • Primerless Glass-to-Metal Bonding
    • Solvent-, Isocyanate-, and PVC-Free Formulation
  • BOSTIK 70-03A

    BOSTIK 70-03A

    • 2.5 MPa Lap Shear
    • Primerless Multi-Substrate Adhesion
    • Up to 120 deg C Service
  • BOSTIK 70-05A

    BOSTIK 70-05A

    • High-Strength Structural SMP Bonding
    • Primerless Multi-Substrate Adhesion
    • UV and Weather Resistance
  • BOSTIK 70-08A

    BOSTIK 70-08A

    • High-Green-Strength SMP Adhesive
    • Primerless Glass Bonding
    • Solvent-, Isocyanate-, and PVC-Free Formulation
  • BOSTIK 940FS

    BOSTIK 940FS

    • 10-Minute Cure Cycle
    • Adhesion and Mechanical Performance of Polyurethane
    • Primerless Glass-to-Aluminum Bonding
  • BOSTIK ISR70-03A

    BOSTIK ISR70-03A

    • Primerless Elastic Silyl-Modified-Polymer Bonding
    • Solvent-, Isocyanate-, and PVC-Free Formulation
    • Transportation and Industrial Assembly Bonding
  • BOSTIK STR350A

    BOSTIK STR350A

    • Elastic Adhesive/Sealant Performance
    • -40 to 121 deg C Service
    • Primerless Multi-Substrate Adhesion
  • DOWSIL 3-6548

    DOWSIL 3-6548

    • Fire-Resistant RTV Silicone Foam
    • 2x to 4x Liquid-Volume Expansion
    • Flexible Medium-Density Ozone/UV-Resistant Foam
  • FREKOTE B-15

    FREKOTE B-15

    • One-Part Polymeric Mold Sealing
    • 30-Minute Recoat Window
    • 24-Hour Full-Cure Sealing
  • FREKOTE FMS

    FREKOTE FMS

    • Composite-Mold Microporosity Sealing
    • High-Gloss Prepared Mold Surface
    • 20-Minute Final-Coat Cure at 20 deg C
  • FREKOTE FMS-100

    FREKOTE FMS-100

    • Room-Temperature Mold-Sealer Cure
    • Microporosity-Sealing Mold Preparation
    • High-Gloss Release-Ready Surface
  • LORD 4688

    LORD 4688

    • Low-Density Honeycomb-Core Syntactic Reinforcement
    • Thixotropic Application Control
    • 30-Minute Working Window
  • 3M 05096

    3M 05096

    • Fine Small-Defect Filling
    • Smooth Feathered Edges
    • Low-Shrinkage Spot Repair
  • 3M 2084

    3M 2084

    • One-Part No-Mix Application
    • Five-Minute Tack-Free Time
    • Flexible Fluid-Resistant Seal
  • 3M 3950

    3M 3950

    • Film Edge-Lift Protection
    • Water-Tight Interface Sealing
    • Defined 50-100 deg F Application
  • 3M 4200FC

    3M 4200FC

    • Fast Moisture-Cure Sealing
    • Non-Sag Marine Application
    • Flexible Bonds for Disassembly
  • 3M ES-2000

    3M ES-2000

    • Clear High-Gloss Edge Seal
    • Controlled 1:1 Duo-Pak Application
    • 25-Minute Tack-Free Time
  • LOCTITE NS5109

    LOCTITE NS5109

    • High-Temperature Flexible Sealing
    • High-Pressure Sealing up to 34 MPa
    • One-Part No-Mix Application
  • PERMABOND TA4246

    PERMABOND TA4246

    • 1-2 Minute Aluminum Fixture
    • 33-35 N/mm2 Steel Shear
    • No-Mix Initiator 46 System
  • PRC-DESOTO PR 1775

    PRC-DESOTO PR 1775

    • Non-Chromate Corrosion Barrier
    • Selectable Class B Work Life
    • Fuel-Exposed Elastomeric Seal
  • PRC-DESOTO PR 1776M

    PRC-DESOTO PR 1776M

    • Low-Density Fuel-Tank Sealing
    • Multi-Grade Class B Work Life
    • Fuel-Resistant Elastomeric Seal
  • PRC-DESOTO PR 870B1/2

    PRC-DESOTO PR 870B1/2

    • Class B-1/2 Processing Window
    • Corrosion-Inhibitive Dissimilar-Metal Seal
    • High-Elongation Cured Seal
  • ROYAL WS-8010

    ROYAL WS-8010

    • Low-adhesion removable gasket
    • Two Class B work lives
    • Low-sag room-temperature cure
  • ROYAL WS-8020RC

    ROYAL WS-8020RC

    • Rapid room-temperature cure
    • Low-sag thixotropic application
    • Fuel and oil resistance
  • ROYAL WS-8032

    ROYAL WS-8032

    • Ultra-lightweight Class B system
    • Fast room-temperature cure
    • Low-sag extrusion handling
  • ROYAL WS-8032S

    ROYAL WS-8032S

    • Ultra-lightweight mixed density
    • Two Class B work lives
    • 360 deg F intermittent exposure
  • ROYAL WS-8035

    ROYAL WS-8035

    • Rapid-cure Class B profile
    • Lightweight cured specific gravity
    • Documented electrical resistivity
  • ROYAL WS-8070

    ROYAL WS-8070

    • Corrosion-inhibitive aerospace sealing
    • Non-sag extrusion handling
    • Two Class B work lives
  • ROYAL WS-8072

    ROYAL WS-8072

    • Selectable B-1/2 and B-2 work lives
    • Non-sag extrusion and spatula application
    • Corrosion-inhibitive aircraft sealing
  • SIKAFLEX 715

    SIKAFLEX 715

    • Semi-Self-Leveling Roof Application
    • 30-Minute Skin Time
    • 500% Cured Elongation
  • 3M 4412N

    3M 4412N

    • 2.0 mm Sealing-Tape Thickness
    • Instantly Paintable Ionomer Backing
    • Immediate Seal Without Chemical Cure
  • 3M 5354

    3M 5354

    • Non-Curing Butyl Sealant Tape
    • Low Moisture-Vapor Transmission
    • Vertical, Overhead, and Corner Placement
  • 3M 800

    3M 800

    • 5 to 10-Minute Tack-Free Time
    • -54 to 93 deg C Service Range
    • Water, Oil, and Fuel Resistance
  • BOSTIK 70-07A

    BOSTIK 70-07A

    • Adjustable Spray-Texture Application
    • Elastic from -40 to 100 deg C
    • Primerless Adhesion on Listed Substrates
  • BOSTIK 940A

    BOSTIK 940A

    • Extended Open Time for Large Applications
    • UV-Resistant Marine Bonding and Sealing
    • Sandable and Paintable After Cure
  • BOSTIK STR220A

    BOSTIK STR220A

    • Elastic SMP Joint Bonding
    • 30-Minute Skin Formation
    • Excellent UV and Weather Resistance
  • BOSTIK STR-350A

    BOSTIK STR-350A

    • Fast 15-Minute Skin Formation
    • High-Elongation Elastic Joint
    • Excellent UV Resistance
  • LOCTITE IS5110

    LOCTITE IS 5110

    • Low-Viscosity Leak-Path Impregnation
    • Water-Rinsable Post-Impregnation Cleanup
    • Anaerobic Sealing Inside Porosity
  • LOCTITE PC6249

    LOCTITE PC 6249

    • No-Mix Epoxy Application
    • Multi-Method Floor Coating
    • At Least 0.8 Wet Friction
  • LOCTITE PC7257

    LOCTITE PC 7257

    • 1:5 Volume Mixing
    • 3 to 11-Minute Initial Set
    • 48 to 55 N/mm^2 28-Day Strength
  • LOCTITE PC9410

    LOCTITE PC9410

    • 3 to 11 Minute Initial Set
    • -25 to 45 deg C Placement Range
    • 17 to 21 N/mm^2 Strength After 2 Hours
  • LOCTITE PC9422

    LOCTITE PC9422

    • 460 mm Maximum Grout Depth
    • 285-Minute Working Life
    • 95 N/mm^2 Cured Compressive Strength
  • LORD 1110

    LORD 1110

    • Low-Density Epoxy Foam
    • Extended Working Time
    • High Compressive Strength
  • PERMABOND TA439

    PERMABOND TA439

    • 20-40 Second Structural Fixture
    • Low-Viscosity 0.15 mm Gap Bonding
    • High Peel and Impact Resistance

Product selector guide

How to select the right polysulfide sealant?

For aerospace sealing applications, select polysulfide sealants based on application method, cure speed, and environmental requirements:

  • Class A: Low-viscosity brush-grade sealants for coating and surface sealing.
  • Class B: Extrusion-grade sealants for fillet sealing and gap filling applications.
  • Class C: Roller-grade sealants designed for large-area fuel tank sealing.
  • Rapid Cure: Selected when reduced processing time is required.
  • Non-Chromate: Preferred where environmental compliance requirements apply.

 

Polysulfide Sealants

Product RTU Type Application Area Grade / Class Application Method Curing Mechanism Color Product Features Specifications
WS-8010 Two-Part (2K) Aircraft access doors, fillet sealing Class B Extrusion / Fillet Chemical Cure at room temperature Black / White General purpose aerospace sealant with excellent adhesion and flexibility AMS3284 Type 1
MIL-S-8784
WS-8020RC Two-Part (2K) Fuel tank sealing, general aerospace sealing Class A Brush Application Rapid Chemical Cure at room temperature Black Rapid cure, high temperature resistance, fuel resistant AMS8802 Type 2
AMS3276
Cessna CPN021 Type 1
WS-8020RC Two-Part (2K) Fuel tank sealing, structural sealing, high temperature applications Class B Extrusion / Gun Grade Rapid Chemical Cure at room temperature Black Rapid curing fuel tank sealant with excellent environmental resistance AMS3276
AMS8802 Type 2
Boeing BMS5-104 Type IV
Boeing BMS3-32 Grade 2
WS-8030 Two-Part (2K) Lightweight fuel tank sealing Class B Extrusion Chemical cure at room temperature White / Gray Lightweight formulation with high temperature resistance AMS3281 Type 1
WS-8031 Two-Part (2K) Lightweight aircraft fuel tank sealing Class B Extrusion Chemical Cure at room temperature White Lightweight sealant designed for aerospace fuel systems AMS3281 Type 3
WS-8032 Two-Part (2K) Fuel tank sealing and aerospace structures Class B Extrusion Chemical Cure at room temperature White Lightweight fuel tank sealant with aerospace qualification AMS3281 Type 2
Korea Aerospace Industries A84MS0022
WS-8032 Two-Part (2K) Fuel tank sealing, roller application Class C Roller Grade Chemical Cure at room temperature White Low viscosity roller grade sealant for large surface application AMS3281 Type 2
Korea Aerospace Industries A84MS0022
WS-8032S Two-Part (2K) Fuel tank sealing, non-chromate applications Class B Extrusion Rapid Chemical Cure at room temperature White Lightweight, rapid cure, environmentally friendly non-chromate formulation Bombardier BAMS552-009
Airbus A2MS552-008
WS-8032S Two-Part (2K) Fuel tank and environmental sealing Class C Roller Grade Chemical Cure at room temperature White Non-chromate roller grade sealant for aerospace applications Bombardier BAMS552-009
Airbus A2MS552-008
WS-8033 Two-Part (2K) Lightweight fuel tank sealing Class B Extrusion Chemical Cure at room temperature White Lightweight aerospace fuel tank sealant Embraer MEP09-084 Grade B Type 1
WS-8035 Two-Part (2K) Fuel tank sealing Class A Brush Grade Rapid Chemical Cure at room temperature Black Fast curing brushable fuel tank sealant Boeing BMS5-184
WS-8035 Two-Part (2K) Fuel tank sealing and general aerospace sealing Class B Extrusion Rapid Chemical Cure at room temperature Black Rapid cure, general purpose aerospace sealant Boeing BMS5-184
WS-8070 Two-Part (2K) Corrosion protection sealing Class B Extrusion Chemical Cure at room temperature Gray Corrosion-inhibitive aerospace sealant MIL-PRF-81733 Class 1 Grade A Type II
Cessna CPN007 Type X
WS-8072 Two-Part (2K) Corrosion protection and environmental sealing Class B Extrusion Rapid Chemical Cure at room temperature Gray Non-chromate, lightweight corrosion inhibitive sealant MIL-PRF-81733 Class 1 Grade B Type II
AMS3265

Frequently asked questions

Frequently Asked Questions about Polysulfide Sealants

What is polysulfide sealant used for?

Polysulfide sealants are used in applications requiring strong chemical resistance, fuel resistance, flexibility, and long-term sealing reliability. They are commonly used for aircraft fuel tank sealing, aerospace structures, marine applications, insulating glass units, expansion joints, automotive sealing, and industrial assemblies exposed to oils, solvents, and harsh environmental conditions.

Is polysulfide better than silicone?

Neither technology is universally better; the right choice depends on the application requirements. Polysulfide sealants generally offer stronger resistance to fuels, oils, solvents, and gases, making them a common choice for aerospace and chemical-exposure applications. Silicone sealants generally offer better UV resistance, wider temperature capability, and stronger long-term weathering performance, making them a common choice for outdoor glazing and high-temperature sealing.

How long does polysulfide sealant last?

A properly selected and applied polysulfide sealant can provide an extended service life, supported by strong resistance to moisture, chemicals, fuel exposure, and temperature cycling that helps it maintain flexibility and sealing performance over time. Actual service life depends on the formulation, substrate compatibility, joint design, environmental exposure, and application conditions, so specific service life expectations should be confirmed against product-specific data.

Can polysulfide withstand aviation fuel?

Yes. Polysulfide sealants are widely recognized for their resistance to aviation fuels, including jet fuel and other hydrocarbon-based fluids. This fuel-resistant property makes polysulfide one of the preferred sealing technologies for aircraft fuel tanks, fuel system components, and aerospace structures where long-term resistance to aggressive chemicals is required.

How does polysulfide sealant cure?

Polysulfide sealants cure through a chemical crosslinking reaction, where the liquid polysulfide polymer reacts with a curing agent to form a flexible, three-dimensional elastomer network. Two-component systems begin curing immediately after mixing, while one-component formulations cure through exposure to environmental conditions, depending on the specific chemistry.

What is the difference between gun grade and pourable polysulfide sealants?

Gun grade polysulfide sealants are higher-viscosity, non-sag formulations designed for vertical, overhead, and controlled bead applications using dispensing equipment. Pourable polysulfide sealants have lower viscosity and are self-leveling, making them suited to horizontal joints, expansion gaps, and large-area sealing applications where complete cavity filling is required.

Are polysulfide sealants waterproof?

Yes. Once fully cured, polysulfide sealants offer strong resistance against water penetration and moisture exposure. Their low permeability and flexible, rubber-like structure help them maintain a reliable seal through weathering, thermal cycling, and prolonged outdoor exposure.


Learn more

Understanding Polysulfide Sealants

Sealant technology engineered for strong chemical resistance, fuel resistance, and long-term environmental durability

Polysulfide sealant chemistry
Chemical Resistant
Synthetic Elastomer

What Are Polysulfide Sealants?

Polysulfide sealants are elastomeric sealing materials based on a liquid polysulfide polymer backbone. They are engineered for applications requiring strong resistance against fuels, solvents, chemicals, moisture, and harsh environmental exposure.

Unlike silicone or polyurethane sealants, which rely on siloxane or urethane chemistry, polysulfides contain repeating sulfur-containing polymer chains that provide low gas permeability and strong resistance to hydrocarbon-based fluids.

During cure, reactive terminal groups crosslink the liquid polymer into a flexible three-dimensional elastomer network, forming a durable seal.

Polysulfide Technology – Key Characteristics
Strong Chemical Resistance

Strong resistance to aviation fuels, oils, solvents, hydraulic fluids, and aggressive chemicals.

Low Gas & Moisture Permeability

The sulfur-based polymer structure provides strong barrier properties against water vapor and gases.

Long-Term Flexibility

Maintains elasticity under temperature cycling, vibration, and continuous mechanical movement.

 

Types of Polysulfide Sealants

Different formulations provide different processing methods, cure profiles, and application performance

 
Single Component 1K

1. One-Component (1K) Polysulfide Sealants

One-component polysulfide sealants are pre-formulated systems supplied ready for application. They cure through exposure to atmospheric moisture or oxygen, depending on the specific formulation chemistry.

These systems offer convenience for field applications where mixing equipment is impractical.

 
Mixed Cure 2K

2. Two-Component (2K) Polysulfide Sealants

Two-component polysulfide sealants consist of a base polymer component and a curing agent that are mixed immediately before application.

The chemical reaction creates a highly crosslinked elastomer with strong mechanical properties, chemical resistance, and long-term durability.

Polysulfide Sealant Application Formats
 
Thixotropic Gun Grade

3. Gun Grade Polysulfide Sealants

Gun grade polysulfides are formulated with higher viscosity and controlled flow characteristics, allowing application through manual or pneumatic dispensing equipment.

The non-sag formulation allows the sealant to hold position on vertical and overhead surfaces while forming a durable elastic seal.

Typical Uses:

Aircraft fuel tank sealing, construction joints, automotive sealing, marine assemblies.

 
Self-Leveling Pourable

4. Pourable Grade Polysulfide Sealants

Pourable polysulfides have lower viscosity and are designed to flow freely into horizontal joints, gaps, and cavities before curing into a flexible rubber seal.

They offer good movement capability and are commonly selected for large-area sealing applications requiring uniform filling.

Typical Uses:

Airport runway joints, expansion joints, insulating glass units, and large structural gaps.

 

Polysulfide Curing Mechanism

The transformation from liquid polymer chains into a durable elastomeric sealing network

Stage 1

Liquid Polymer Before Cure

The polysulfide polymer exists as a flexible liquid chain containing reactive terminal groups. At this stage, the material remains flowable and can wet the substrate surface.

Stage 2

Crosslinking Reaction

The curing agent reacts with terminal functional groups, connecting individual polymer chains into a growing three-dimensional network.

Stage 3

Fully Cured Elastomer

The completed crosslinked rubber structure provides flexibility, chemical resistance, low permeability, and long-term sealing performance.

Key Performance Benefits

Why polysulfide sealants are a common choice for demanding sealing environments

 

1. Fuel & Chemical Resistance

Hydrocarbon Resistance: The sulfur-containing polymer structure provides strong resistance against aviation fuels, diesel, gasoline, hydraulic fluids, and lubricants.

Chemical Stability: Maintains sealing integrity when exposed to solvents, oils, cleaning agents, and industrial chemicals.

 

2. Environmental Durability

Weather Resistance: Strong resistance against UV exposure, ozone, humidity, and temperature cycling.

Extended Service Life: Formulated to maintain elasticity and sealing performance over long operating periods in demanding outdoor environments; actual service life depends on formulation, substrate, joint design, and exposure conditions.

 

3. Movement Capability

Elastic Recovery: The flexible polymer network allows repeated expansion and contraction without cracking.

Stress Absorption: Accommodates thermal expansion differences between dissimilar substrates.

 

4. Low Gas & Moisture Permeability

Barrier Protection: The dense sulfur-based polymer structure minimizes gas transmission and moisture penetration, which is why polysulfides are a common choice for fuel tanks, aerospace sealing, and insulating glass applications.

 

Core Industrial Applications

Polysulfide sealants are selected where long-term sealing reliability and chemical resistance are critical

Industry Application
Aerospace & Aviation Aircraft fuel tank sealing, fuselage joints, access panels, and aerospace structures requiring resistance to aviation fuels and hydraulic fluids.
Automotive & Transportation Fuel system sealing, vehicle body joints, industrial equipment sealing, and applications exposed to oils and chemicals.
Marine & Shipbuilding Deck joints, marine structures, underwater sealing, and applications requiring saltwater and weather resistance.
Construction Expansion joints, concrete sealing, building facades, and structural gaps exposed to movement.
Insulating Glass Secondary seal applications requiring low moisture and gas permeability.
 

Polysulfide vs Other Sealant Technologies

General positioning across three common sealant chemistries. Actual performance varies by specific formulation and test conditions, so product-specific data should be checked before final selection.

Property Polysulfide Silicone Polyurethane
Fuel Resistance Strong Limited Moderate
UV Resistance Good Strong Good
Gas Permeability Strong barrier Moderate Moderate

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers